Effect of desizing treatment on carbon fiber properties and performance in carbon–carbon composite rocket nozzle / Ryszard WIELOWSKI, Maciej GUBERNAT, Marcel ZAMBRZYCKI, Piotr JELEŃ, Zofia KUCIA, Norbert MOSKAŁA, Krystian SOKOŁOWSKI, Aneta FRĄCZEK-SZCZYPTA // Composites ; ISSN 1359-835X . Part A, Applied Science and Manufacturing ; ISSN 1359-835X. — 2027 — vol. 212 art. no. 110288, s. 1–14. — Bibliogr. s. 13–14, Abstr. — Publikacja dostępna online od: 2026-09-17
Autorzy (8)
Słowa kluczowe
Dane bibliometryczne
| ID BaDAP | 170741 |
|---|---|
| Data dodania do BaDAP | 2026-11-08 |
| Tekst źródłowy | URL |
| DOI | 10.1016/j.compositesa.2026.110288 |
| Rok publikacji | 2027 |
| Typ publikacji | artykuł w czasopiśmie |
| Otwarty dostęp | |
| Creative Commons | |
| Czasopismo/seria | Composites, Part A, Applied Science and Manufacturing |
Abstract
This study investigates the influence of thermal desizing on the surface, structural, and mechanical properties of PAN-based carbon fibers for carbon–carbon composite applications. Fibers were heat-treated in nitrogen between 25 and 900 °C and characterized using SEM, AFM, Raman spectroscopy, XPS, TOF-SIMS, contact angle measurements, and tensile testing. Effective removal of the epoxy sizing layer occurred at approximately 400 °C, producing a clean surface with minimal damage and the lowest roughness. Higher temperatures (700-800 °C) increased roughness and defect density due to surface degradation and carbonaceous residue formation, while partial surface cleaning reappeared at 900 °C. Raman analysis confirmed that the bulk fiber structure remained largely unchanged, indicating predominantly surface-related modifications. Surface chemistry evolved from epoxy-dominated to graphitic sp2-rich above 400 °C, whereas TOF-SIMS detected residual epoxy species up to ∼ 520 °C. Tensile tests revealed moderate strength reduction after desizing and significant degradation above 600 °C. Composites fabricated with fibers desized at 500 °C exhibited improved performance, with interlaminar shear strength increasing by up to 44 %. The optimal desizing window was identified as 400-500 °C, providing a balance between sizing removal, surface quality, and mechanical performance for composite rocket nozzle applications. © 2026 The Author(s).