Structure evolution and bonding inhomogeneity toward high thermoelectric performance in $Cu_{2}CoSnS_{4–x}Se_{x}$ materials / Taras PARASHCHUK, Oleksandr CHERNIUSHOK, Oleksandr Smitiukh, Oleg Marchuk, Krzysztof T. WOJCIECHOWSKI // Chemistry of Materials ; ISSN 0897-4756. — 2023 — vol. 35 iss. 12, s. 4772–4785. — Bibliogr. s. 4783-4785, Abstr. — Publikacja dostępna online od: 2023-06-07

Autorzy (5)

Dane bibliometryczne

ID BaDAP147559
Data dodania do BaDAP2023-07-27
Tekst źródłowyURL
DOI10.1021/acs.chemmater.3c00586
Rok publikacji2023
Typ publikacjiartykuł w czasopiśmie
Otwarty dostęptak
Creative Commons
Czasopismo/seriaChemistry of Materials

Abstract

Lightweight diamond-like structure (DLS) materials are excellent candidates for thermoelectric (TE) applications due to their low costs, eco-friendly nature, and property stability. The main obstacles restricting the energy-conversion performance by the lightweight DLS materials are high lattice thermal conductivity and relatively low carrier mobility. By investigating the anion substitution effect on the structural, microstructural, electronic, and thermal properties of Cu2CoSnS4–xSex, we show that the simultaneous enhancement of the crystal symmetry and bonding inhomogeneity engineering are effective approaches to enhance the TE performance in lightweight DLS materials. Particularly, the increase of x in Cu2CoSnS4–xSex makes the DLS structure with the ideal tetrahedral bond angles of 109.5° favorable, leading to better crystal symmetry and higher carrier mobility in samples with higher selenium content. In turn, the phonon transport in the investigated DLS materials is strongly disturbed due to the bonding inhomogeneity between anions and three sorts of cations inducing large lattice anharmonicity. The increase of Se content in Cu2CoSnS4–xSex only intensified this effect resulting in a lower lattice component of the thermal conductivity (κL) for Se-rich samples. As a result of the enhanced power factor S2ρ–1 and the low κL, the dimensionless thermoelectric figure of merit ZT achieves a high value of 0.75 for Cu2CoSnSe4 DLS material. This work demonstrates that crystal symmetry and bonding inhomogeneity play an important role in the transport properties of DLS materials and provide a path for the development of new perspective materials for TE energy conversion.

Publikacje, które mogą Cię zainteresować

artykuł
#141500Data dodania: 31.8.2022
Lone-pair-like interaction and bonding inhomogeneity induce ultralow lattice thermal conductivity in filled β-manganese-type phases / Oleksandr CHERNIUSHOK, Raul Cardoso-Gil, Taras PARASHCHUK, Rafał KNURA, Yuri Grin, Krzysztof T. WOJCIECHOWSKI // Chemistry of Materials ; ISSN 0897-4756. — 2022 — vol. 34 iss. 14, s. 6389-6401. — Bibliogr. s. 6400-6401, Abstr. — Publikacja dostępna online od: 2022-05-27
artykuł
#134585Data dodania: 14.6.2021
Engineering electronic structure and lattice dynamics to achieve enhanced thermoelectric performance of Mn−Sb co-doped GeTe / Ashutosh Kumar, Preeti Bhumla, Taras Parashchuk, Stanisław Baran, Saswata Bhattacharya, Krzysztof T. WOJCIECHOWSKI // Chemistry of Materials ; ISSN 0897-4756. — 2021 — vol. 33 iss. 10, s. 3611–3620. — Bibliogr. s. 3618–3620, Abstr. — Publikacja dostępna online od: 2021-05-11